    US-Made Batteries w/ Atomic Layer Deposition Enter Space

    08/17/2021
    US-made batteries containing Forge Nano's proprietary Particle Atomic Layer Deposition (PALD) nanotechnology have launched into space….

    Forge Nano is proud to announce the successful launch of high-energy, Lithium-ion (Li-ion) batteries into orbit aboard the SpaceX Transporter-2 rideshare mission on June 20, 2021. The Li-ion batteries, featuring Forge Nano Particle ALD (PALD) technology and Enersys Zero Volt technology, were integrated into Spire Global, Inc.'s LEMUR-2 satellite. The batteries used 100 percent domestically sourced electrode materials from Pyrotek and Forge Nano. 

    Paul Lichty, CEO of Forge Nano, explains "This is the first ALD-enabled space battery we know of and it's mostly made with US materials! As world leaders in battery materials, we're excited to be pushing limits of performance for various applications including space. This partnership with EnerSys, Pyrotek, and Spire Global is just one of many commercial battery projects we're working on, and we look forward to sharing these other projects with the world soon."

    Forge Nano's Particle Atomic Layer Deposition (PALD) technology, developed by Forge Nano founders while at the University of Colorado Boulder, allows batteries to survive longer and perform better across a variety of metrics. PALD is applicable and cost-effective for most cathodes, anodes, separators, and solid-state battery materials. Forge Nano works with companies from across the globe to enhance their materials with PALD.

    The battery cells sent to space incorporated domestically sourced anode material from Pyrotek, headquartered in Spokane, Washington, and cathode material from Forge Nano. Both electrode materials utilized Forge Nano's Particle Atomic Layer Deposition (PALD) coatings and combined with EnerSys ZeroVolt technology to enhance cycle life stability, energy density, and low temperature performance. The batteries were sent to space aboard a Spire Global, Inc. LEMUR-2 satellite and will be electrically cycled in-orbit at specific Depth of Discharge (DOD) levels to determine their electrical performance in a space environment as part of the battery qualification process.

    "By integrating the various parties' technologies into Spire's LEMUR-2 satellite, we are able to gather relevant performance data in a spaceflight application and advance the use of this technology more broadly within the space industry." said Keith E. Johnson, Vice President and General Manager, Federal at Spire Global, Inc.

    "These new US-made batteries pave the way for a fully integrated US battery supply chain at a critical time in the domestication of the battery industry," said Mark Matthews, EnerSys Senior Vice President, Specialty – Global.

    For more information, visit Forge Nano, Spire Global, Enersys, and Pyrotek.

    Related

    Power Systems Design

    146 Charles Street
    Annapolis, Maryland 21401 USA

    Power Systems Design

    Power Systems Design is a leading global media platform serving the power electronics design engineering community. It delivers in-depth technical content, industry news, and product insights to engineers and decision-makers developing advanced power systems and technologies.

    Published 12× per year across North America and Europe, Power Systems Design is distributed through online and fully digital editions, complemented by eNewsletters, webinars, and multimedia content. The platform covers key areas including power conversion, semiconductors, renewable energy, automotive electrification, AI power systems, and industrial applications—supporting innovation across the global electronics industry.